ASTM B861 25*1.2mm Titanium Tube For Chemicals are generally divided into two types, one is the extruded type called seamless titanium tube; the other is welded type called welded titanium tube.
1. If it is semi-automatic cutting, the guide rail should be placed on the titanium tube plane, and then the cutting machine should be placed on the guide rail, and the order should not be reversed.
2. The cutting parameters should be appropriate, and should be reasonably determined according to the thickness of the titanium heat exchanger tubing, so as to obtain a good cutting effect.
3. Check whether the cutting gas is unobstructed. If there is a blockage, it should be unblocked in time.
4. Before cutting, the surface should be cleaned and some space should be left, which can facilitate the blowing out of slag.
5. The distance between the cutting nozzle and the surface of the titanium tube should be appropriate, too close or too far is not good.
6. Preheating should be sufficient so as not to affect the cutting process.
7. If cutting workpieces of different sizes, the small ones should be cut first, and then the large ones.